A New Approach To Glass Furnace Repair: Ceramic Welding Below The Glass Line

An account is given on a repair on a container furnace at Latchford Glass's Los Angeles plant at which an area below the flux line at the back wall was welded, as well as along both sidewalls.

Author
T R Busby
Origin
Fosbel Inc
Journal Title
American Glass Review December 1989 8-9