Nature Of Energy Of Activation And Experimental Data On The Fluiduty Of Refracotry Glass-Forming Substances.

The energies of the chemical valence of silicon oxide and boron oxide indicate that valence bond rupture is incapable of being an important part of structural processes, of fusion and of crystallisation. A postulate has been advanced as to possible structural regrouping of atom and shrifts in relative potions by switches in the chemical valence bonds between atoms.

Author
R.L. Myullet
Origin
Unknown
Journal Title
Chemistry Collection No.2, Soviet Research In Glass & Ceramics, Basic Science Ii. Pp. 457.463
Sector
Primary Papers
Class
PP 720

Request article (free for British Glass members)

Nature Of Energy Of Activation And Experimental Data On The Fluiduty Of Refracotry Glass-Forming Substances.
Chemistry Collection No.2, Soviet Research In Glass & Ceramics, Basic Science Ii. Pp. 457.463
PP 720
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.