Multiple Section Is Machine Concept

Based on a paper presented at Glassman America 96, this paper reviews the preconditions which have to be fulfilled to operate high speed forming equipment for lightweight glass containers. A comparison between multi-section and multi-gob machines is included, together with experiences from existing production lines.

Author
H Griffel
Origin
Heye-Glas, Germany
Journal Title
Glass 73 5 1996 173-174