Multi-Touch Screen Development

In order to respond to the increasing demand for touch cover screens using FTIR (Frustrated Total Internal Reflection) technology, AGC has launched TIREXtreme glass. Pioneers in the development of this promising infrared in glass multi touch detection like FlatFrog have already adopted the development for screens measuring over 20in. They were won over by its exceptional transmission power in the near infrared (780-1500 nanometers). While offering the same aesthetic properties as clear glass, TIRExtreme has near infrared absorption up to 30 times lower than extra-clear float glass, thanks to its special composition. These characteristics, combined with its affordable costs, make the product an excellent material for any technology that depends on the transmission of IR through a transparent structure. For more information, please visit: www.agc-glass.eu

Author
A Ribesse
Origin
Agc Europe
Journal Title
Glass Worldwide Nov-Dec 2015 134
Sector
Flat glass
Class
F 3756

Request article (free for British Glass members)

Multi-Touch Screen Development
Glass Worldwide Nov-Dec 2015 134
F 3756
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.