Monitoring Temperatures In Glass Bending Furnaces

This article discusses the application of an Infrared Line Camera in the production process of windshields. For example, glass that is used as windshield has to be bent. Common bending principles include the bending by press bending or gravitation. The glass panes are placed on the hoop and then heated in the bending furnace. The glass nestles to the hoop and attains the desired form. This article can be read online for free from: www.azom.com/article.aspx?ArticleID=14151