Modular Spray System Cuts Costs And Waste

Shear sprays are a vital part of the lubrication system in any container plant. They can also be the source of many problems. This article describes a one-way system which solves many of the common problems by removing the need for a solution/emulsion holding tank. It is also modular, allowing a customised installation to be built from standard units.