Modern Technologies For Protecting The Environment From Wastes Of The Glass Industry

A way to create resource and power-saving technological processes, equipment, and plants that meets modern ecological requirements is suggested. The engineering solutions have been successfully tested and installed in some enterprises.

Author
V G Kalygin
Origin
Moscow State Acad Chem Eng, Russia
Journal Title
Glass & Ceramics 53 1-2 1996 1-5
Sector
General
Class
G 1985