Modelling, Design And Implementation Of A Servo-Electric Plunger Mechamism For Glass Container Forming Machines

Within the scope of increasing the reliability, the controllability and the speed of glass container forming machines and thus improving the related forming process, servo-electric drives are increasingly replacing pneumatically driven mechanisms that still represent the standard in IS machines today. This paper discusses the design and the results of an experimental unit of a fully functional servo-electric plunger mechanism, developed by Emhart Glass SA.

Author
W Gruninger Et Al
Origin
Emhart, Switzerland
Journal Title
Glass Technology 43 3 June/02 89-94
Sector
Container glass
Class
C 2152

Request article (free for British Glass members)

Modelling, Design And Implementation Of A Servo-Electric Plunger Mechamism For Glass Container Forming Machines
Glass Technology 43 3 June/02 89-94
C 2152
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.