Micro-Alloys Precipitation In Nio- And Coo-Bearing Enamel Coatings And Their Effect On Adherence Of Enamel/Steel

The effect of CoO and NiO on the adherence between enamel coating and steel is being investigated experimentally in this study. Enamel coatings are applied to the steel using a wet process with slurries. A total fo five enamels were prepared including three single layer enamels: blank enamel; NiO bearing enamel; CoO bearing enamel; and two double layer enamels - BL-MTNi3, BL-MTCo3, which consisted an inner layer of BL and an outer layer of MTNi3 or MTCo3. Falling-weights test were performed and the cross-sections at the enamel/steel interface were analysed with SEM coupled with an energy dispersive spectroscopy (EDS) and electron probe micro-analysis. Results show that the increases of adherence for MTCo3 and MTNi3 coated steel are attributed to the micro-alloys precipitation at the enamel/steel interface.

Author
K Chen Et Al
Origin
University Sci & Technol, Hefei, China
Journal Title
Int J Appl Glass Sci 9 1 2018 70-84
Sector
Enamels
Class
E 171

Request article (free for British Glass members)

Micro-Alloys Precipitation In Nio- And Coo-Bearing Enamel Coatings And Their Effect On Adherence Of Enamel/Steel
Int J Appl Glass Sci 9 1 2018 70-84
E 171