Methods For Determining The Flow In Glass Tanks. A Literature Review.

Methods for determining the flow in glass tanks described in the literature are reviewed, in particular float measurement, and float measurement by means of mechanical apparatus in the glass bath. Methods must be developed for measuring any velocity vectors in the glass bath.