Methods And Measures

The measures adopted by Schott for scrubbing waste gases and the filter equipment used on the furnaces in their various plants are described briefly. Methods for dealing with other types of industrial pollution are also discussed.

Author
H-G Otto
Origin
Schott Glaswerke
Journal Title
Schott Information 1987 4 3-7
Sector
General
Class
G 134

Request article (free for British Glass members)

Methods And Measures
Schott Information 1987 4 3-7
G 134