Melting Sensor Needs Identified

There are numerous commercial, off-the-shelf sensors and measurement systems in use on modern glass melters. All are typically characterised by their ability to operate in a harsh service environment with minimal maintenance. This article discusses potential improvements to existing sensors that could help with sustainability of the glass industry, while also focusing on developments that could improve melter operation, glass quality and industry competitiveness.

Author
D A Gaerke
Origin
O-I Usa
Journal Title
Glass Worldwide Jan-Feb 2016 58, 60, 62