FIC, based in Penzance, Cornwall, claims to be the first in the glass industry to have been accredited with the ISO 9001 standard for the design and manufacture of its all-electric glass melting and boosting systems. Amongst the wide range of products which FIC manufactures are electric melting systems which offer the benefits of increased pull rate, reduction in pollutin emissions, improved glass quality, and a longer furnace life in both float and container glass processing. The company has successfully designed, manufactured, installed and commissioned 11 float line boosting systems around the world.