Mechanical Properties Of Silica Glass Made By The Sol-Gel Process

Mechanical properties such as flexural strength and fracture toughness have been measured experimentally on silica glass samples produced by the company novara technology using the sol-gel method. The aim of this work is to compare these results with data from literature regarding silica glasses produced by melting in order to see how the production process affects the mechanical performance of glasses having the same composition.

Author
M Aielli & Etal
Origin
Italy
Journal Title
Glass Machinery Plants And Accessories July/Aug 2006 83-85
Sector
Special Glass
Class
S 3137

Request article (free for British Glass members)

Mechanical Properties Of Silica Glass Made By The Sol-Gel Process
Glass Machinery Plants And Accessories July/Aug 2006 83-85
S 3137
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.