Measuring Physical Properties Of Glass In The Glass-Transition Region

Three apparent paradoxes in the behaviour of glass in the transition range are discussed. The data were first presented by Lillie, Zijlstra and Larsen respectively.

Author
S M Rekhson
Origin
Ge Lighting
Journal Title
Ceramic Bulletin 1989 68 11 1956-1962
Sector
General
Class
G 337

Request article (free for British Glass members)

Measuring Physical Properties Of Glass In The Glass-Transition Region
Ceramic Bulletin 1989 68 11 1956-1962
G 337