Measuring Nanotechnology

Micro Materials in the UK, claims to have developed the NanoTest modular platform system specifically to meet the challenge of quantitative materials testing at the nano-and micro-scale for research, development and production. The system was designed to support the company's three main nanoscale testing techniques of indentation, scratching and impact. Its design gives users the versatility to construct a comprehensive materials testing centre dedicated to their specific needs. For more information please see: www.micromaterials.co.uk