Measured Angular Distribution Of The Emissivity And Calculated Radiation Heat Transfer Of Architectural Coated Flat Glass

A theoretical and experimental study of the angular variation of total directional emissivity at room temperature of uncoated float glass and typical architectural coatings is reported. The possibility of mathematically correlating the normal with hemispherical and effective emissivity for different materials is discussed.

Author
F Geotti-Bianchini, J Lohrengel
Origin
Stazione Sper Del Vetro, Phys-Techn Bundesanstalt Braunschweig
Journal Title
Glastech Ber 1989 62 9 312-319
Sector
Flat glass
Class
F 166

Request article (free for British Glass members)

Measured Angular Distribution Of The Emissivity And Calculated Radiation Heat Transfer Of Architectural Coated Flat Glass
Glastech Ber 1989 62 9 312-319
F 166
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.