Making Efficient Use Of Glass Cullet

French company Andrin SA, has been manufacturing magnetic handling and lifting equipment for the steel industry for over 40 years. The company has recently developed an Eddy current separator, type "STS", which is close to eliminating 100% of all ferrous and non-ferrous metals contained in cullet.