A Major Step Towards Zero Waste

Changes in lifestyle are leading to increasing demands for disposable goods at the cost of environmentally hazardous fly ash being produced through waste incineration. But the use of plasma vitrification to create fly ash glass can offer an economical and ecological solution.

Author
D Pineau
Origin
Europlasma
Journal Title
Glass Prod Tech Int 1999 10, 12
Sector
General
Class
G 2059