Machine Dishwashing Of Glass In Private Households - Research Results On Glass Damage

Glasses of different origins and compositions were subjected to a continuous dishwashing test with up to 1000 cycles which compared the highly alkaline conventional detergent with different new formulation variants of low-alkaline compact detergent. While the conventional and carbonate-containing compact detergent did not cause visible corrosion, the detergent with a high disilicate content already caused serious damage after 50 washing cycles in the form of clouding and iridescence.

Author
W Buchmeier Et Al
Origin
Henkel Kgaa, Germany
Journal Title
Glastech Ber Glass Sci Technol 69 6 1996 159-166
Sector
Domestic glass
Class
D 260

Request article (free for British Glass members)

Machine Dishwashing Of Glass In Private Households - Research Results On Glass Damage
Glastech Ber Glass Sci Technol 69 6 1996 159-166
D 260
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.