Luminescence Of 5D3 And 5D4 Levels Of Tb3+ In Borate, Phosphate, And Tungstate Glasses Excited By Cathode Rays As A Possible Tool For The Study Of Surface Fluorescence In Glasses.

Borate, phosphate and tungstate glasses doped by Gd3+, and Tb3+, and Eu3+ were excited by cathode rays.

Author
I.J. Brandstadter Et Al
Origin
Unknown
Journal Title
Solid St Commun., 1972, 11 (9) 1235-8
Sector
Primary Papers
Class
PP 750

Request article (free for British Glass members)

Luminescence Of 5D3 And 5D4 Levels Of Tb3+ In Borate, Phosphate, And Tungstate Glasses Excited By Cathode Rays As A Possible Tool For The Study Of Surface Fluorescence In Glasses.
Solid St Commun., 1972, 11 (9) 1235-8
PP 750
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.