[Lubricants] Condat: Experience And Expertise In Development, Manufacturing And Trading

When it was first established 160 years ago, Condat had absolutely no connections with the glass industry. Its roots, in fact, were with the mechanical industry and the machines that were developed in that period. However, today, this French company provides lubricants for both sectors of the glass industry, hollow and flat, and in this article gives an idea of what it supplies and how these products are used.