Low Melting Pbo-Zn0-P205 Glasses. Part 2. A Structural Study By Raman Spectroscopy And Mas-Nmr

The short range structure of a series of low melting lead zinc phosphate glasses containing 30-50 mol% P205, 0-60% PbO and 0-60% ZnO were characterised by Raman spectroscopy and magic angle spinning-nuclear magentic resonance (MAS-NMR) spectroscopy.