The results of synthesis of low-melting matte glazes in the R20-RO-B203-Al203-Ti02-Si02 system are presented. The relationship between the physicochemical properties of the coatings,the phase composition, and the structure of the glazed glasses is investigated as a function of the heat treatment regime.