Low-E Glass Coatings Reduce Energy Consumption

Arkema Inc, is at the forefront of the growing residential & commercial world market for low-E energy efficient glass. The Certincoat CVD System is an online coating technology that is integrated directly into the float glass manufacturing process. Designed for optimum performance, the world's first commercial turnkey online CVD system is easier to install & integrate than a sputtered system & results in lower operating costs as well. Arkema developed the system to bring online pyrolytic coating technology to a broader audience.Many countries do not currently possess the infrastructure, capital & skills required to process sputtered low-E glass into residential & commercial windows. Glass makers do not need any prior CVC knowledge as the system is installed & all appropriate personnel are trained in operation by Arkema's experts.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 1/2006 53
Sector
Flat glass
Class
F 2023

Request article (free for British Glass members)

Low-E Glass Coatings Reduce Energy Consumption
Glass-Tech Int 1/2006 53
F 2023
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.