Lonox Melter Shows Promise

The furnace developed by Sorg to meet pollution emission limits without add-on controls and without sacrificing melting or energy performance is described. Measurements on the first installation, at Weigand Glas, Steinbach, showed that emissions of sulphur and nitrogen oxides were well below the German federal standard values.

Author
R H Moore
Origin
Teichmann/Sorg Group Ltd
Journal Title
Glass Industry March 1990 14-18
Sector
General
Class
G 388

Request article (free for British Glass members)

Lonox Melter Shows Promise
Glass Industry March 1990 14-18
G 388
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.