Liquid crystal displays (LCDs) have now been avialable in the electronics market for 20 years. The first LCDs produced were small, as they were used for watches, calculators and radios. This article reviews the current investment situation for the further development of LCDs and discusses the use of direct heated platinum systems for the production of thin sheet glass for this market.