On-Line Inspection Of Plates And Primary Blanks

A variety of visual gauging and inspection functions must be carried out on plates and primary blanks on the main float line and on secondary lines. SIPA camera-based inspection technology offers powerful on-line systems for size and contour checks, fault marks and defect detection, thus helping to ensure significant improvements in product quality and line productivity.