Limitation Of Griffith Flaws In Glass-Matrix Composites.

The effect of the limitation of Griffith flaws, introduced in an abraded surface of glass, on the strength of glass-tungsten composites was investigated for small sizes of Griffith flaws. Hasselman and Fulrath propsed fracture theory for this type of system extended to small flaw sizes. The use of tungsten spheres with two particle sizes or a wide distribution about one average size as the dispersed phase in a glass matrix decreased the average mean free path in the matrix more than could be achieved with a single particle size dispersion. Average mean paths determined experimentally by statistical techniques were in good agreement with those calculated by Fullman's equation.

Author
Y. Nivas And R.M. Fulrath
Origin
Unknown
Journal Title
J. Am. Ceram. Soc,. 1970, 53 (4), 188-91)
Sector
Primary Papers
Class
PP 352

Request article (free for British Glass members)

Limitation Of Griffith Flaws In Glass-Matrix Composites.
J. Am. Ceram. Soc,. 1970, 53 (4), 188-91)
PP 352
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.