Lightweight Glass Packaging And Pre Labelling Are Hot Items (Dutch)

Trends in glass packaging in the Netherlands and Europe generally are discussed with reference to recycling statistics. The use of recycled cullet by PLM and Vereenigde Glasfabrieken NV in particular is reviewed.