Lighting Considerations In Cut Plate Inspection

Long-term planning should be an important factor in cost considerations, with float lines typically expected to last 12-15 years between rebuilds. In this paper the authors explore how this affects lighting for automated inspection tasks.

Author
F Birchenough & G Farrell
Origin
Ispection Systems Ltd, Uk
Journal Title
Glass Int Nov/Dec 2001 37
Sector
Flat glass
Class
F 1283