The Ligand Field Theory And Optical Properties Of Soda-Lime Glasses (French)

A study of the optical properties of the main colouring elements in commercial soda-lime glasses has led to a new interpretation of the tetrahedral iron (III) spectra and improved attribution of absorption bands in the near infra-red in the case of the optical spectra of nickel glasses.