Lema: Chemical Vs Thermal Tempering In Particualr Shapes And Small Thicknesses Of Glass

In this article, Lema Srl, with over 30 years' experience in the chemical tempering of glass, and the first manufacturer of equipment for this application, explains the process involved. Properties of chemically tempered glass are given, along with recommendations to reduce the risk of ruining glass or the bath.