Leachability Of Molybdenum From Ternary Phosphate Glasses

With a view to use glasses as a source of molybdenum, which is one of the micronutrients required by plants, a systematic study of the leachability of molybdenum from ternary phosphate glasses having molar compositions of 25Mo03.25X.50P205 (where X = Li20, Na20, K20, CaO, B203, or Si02) was carried out

Author
R Pyare Et Al
Origin
Banaras Hindu University, India
Journal Title
J Am Ceram Soc 79 5 1996 1329-1334