Latest Dimension In Container Finish Inspection

In this article the author presents an off-line inspection tool, developed for the precise measurement of critical dimensions associated with the roll-on pilfer-proof finish (ROPP).

Author
G Reid
Origin
Pro-Sight Vision, Uk
Journal Title
Glass Worldwide Jan-Feb 2019 30-31
Sector
Container glass
Class
C 6081

Request article (free for British Glass members)

Latest Dimension In Container Finish Inspection
Glass Worldwide Jan-Feb 2019 30-31
C 6081