Laser Machines For Glass Applications

Neuma Laser supplies the glass industry with laser machines for glass processing and decorating. These modern machines are equipped with a CO2 laser, a gas laser whose beam energy can be easily concentrated on a point and used for cutting, engraving and soldering, The two types of laser machines offered by the Italian manufacturer are the Cartesian model for cutting, and the polar machine, which is particularly suitable for decorating.