The Korean Glass Industry

During the last few years the Korean flat glass industry has grown steadily at an approximate rate of 13% annually, while the glass bottle industry has grown at a 3% rate.

Author
M Pinetti
Origin
Unknown
Journal Title
Glass Machinery Plants & Accessories No 3 1995 79-80, 82
Sector
General
Class
G 1241