Judd-Ofelt Parameters And Radiative Properties Of Pr3+ Ions In Cadmium Borate Glasses

Judd-Ofelt parameters for Pr3+ ions in alkali cadmium borate and alkaline cadmium borate (RCdB, R=Li, Na, K and Mg, Ca, Ba) were derived from the intensities of the integrated absorption bands.