Itrpv 4Th Edition Review: Materials Matter

Over the past two years, the photovoltaic industry has been in disarray as massive global overcapacity has sent prices tumbling. In this context, technological innovation to reduce the costs of base materials and products has become increasingly important. The latest edition of the International Technology Roadmap for PV published in March 2013 offers insights into the latest developments as manufacturers continue to seek ways of cutting costs. This paper explains some of the key dynamics identified in the roadmap.

Author
M Osborne
Origin
Editor, Photovoltaics International
Journal Title
Pv International May 2013 19-21
Sector
Flat glass
Class
F 3435

Request article (free for British Glass members)

Itrpv 4Th Edition Review: Materials Matter
Pv International May 2013 19-21
F 3435
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.