Investigations Concerning The Recycling Of Filter Dust From Electrostatic Precipitators In The Glass Industry

In the container glass industry the recycling of filter dust was applied from the beginning of the waste gas treatment - first mainly in flint glass furnaces. This paper reports on the experiences concerning handling, dusting and refining behaviour. Moreover, the results of a research programme, investigating the danger of enrichment with toxic components in the molten glass, in the filter dust and in the residual emission are presented.

Author
U Kircher
Origin
Huttentechnische Vereinigung Der Deutschen Glas (Hvg), Germany
Journal Title
Glastech Ber 66 11 1993 279-283
Sector
Container glass
Class
C 616

Request article (free for British Glass members)

Investigations Concerning The Recycling Of Filter Dust From Electrostatic Precipitators In The Glass Industry
Glastech Ber 66 11 1993 279-283
C 616
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.