Investigation Of The Process Of Drawing Glass Fibres (German)

The relationship between temperature changes in the onion and the rate of drawing of glass fibre is discussed with the aim of developing a thermal and rheological mathematical model.

Author
M. Stehle And R. Bruckner.
Origin
Unknown
Journal Title
Proc. Of The Xith International Congress On Glass, Prague 1977, V 159-168