Investigation Of The Effect Of Fluorides On Vitrification And The Properties Of Fluo-Alumino-Phosphate Glasses.

A study has been made to select fluorides which could be used to produce phosphate glasses with a high disperation.

Author
L.N. Urusovskaya
Origin
Pilk Trans.
Journal Title
Zh. Prikl. Khim. 1968 41 (11) Pp. 2361-2367
Sector
Primary Papers
Class
PP 856

Request article (free for British Glass members)

Investigation Of The Effect Of Fluorides On Vitrification And The Properties Of Fluo-Alumino-Phosphate Glasses.
Zh. Prikl. Khim. 1968 41 (11) Pp. 2361-2367
PP 856