The Introduction Of Float Glass To China

The history of the float glass process is summarised with particular reference to its introduction by the joint venture company, Shanghai Yaohua Pilkington Glass Co. Ltd. The factory was opened on 6th May, 1988 and has an annual capacity of 200 000 tonnes.

Author
I Bishop
Origin
Unknown
Journal Title
Tin And Its Uses 1988 158 6-7
Sector
Flat glass
Class
F 84

Request article (free for British Glass members)

The Introduction Of Float Glass To China
Tin And Its Uses 1988 158 6-7
F 84