[Interview] Flat Glass - Past, Present And Future

As a provider of system solutions for the manufacture of architectural and automotive glass, Bystronic Glass has a global sales and service network and is present in every important marketplace. In this article Richard Jakob, CEO of Bystronic Glass talks about how the different flat glass sectors have fared during the economic crisis, while looking to the future for new opportunities that recovery will bring.