On The Interaction Between Oxygen, Iron And Sulphor In Industrial Glass Melts

The oxidation state of iron in industrially molten glasses has been investigated in the cold glass and related to the oxygen activity in the glass melt.

Author
H Muller-Simon
Origin
Hvg, Germany
Journal Title
Glastech Ber Glass Sci Tech 67 11 1994 297-303
Sector
General
Class
G 1170

Request article (free for British Glass members)

On The Interaction Between Oxygen, Iron And Sulphor In Industrial Glass Melts
Glastech Ber Glass Sci Tech 67 11 1994 297-303
G 1170