[Inspection] Wire Edge Measurement (Wem): A Multi4 Detection On The Way To Success

This article discusses a detection system dedicated to exposing wire-edge and overpressed flaws.

Author
D Freydiere
Origin
Tiama, France
Journal Title
Glass International April 2019 35-36
Sector
Container glass
Class
C 6150