Inspection Systems For Automotive And Solar Glasses

Available from ISRA Vision is a system for optical 100% in-line silkscreen print inspection, in particular for automotive glasses. Ludger Wahlers presents the Printscan System, along with the company's latest optical inspection systems for solar glass production lines.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Sept/Oct 2010 36-37
Sector
Flat glass
Class
F 2986