Innovative Solutions For Screen Treatment

The belief that there is potential to optimise processes and costs in the screen treatment industry has led to the development of an inclined filter cleaning system for in-house cleaning processes.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide 2 2005 18-19