Innovation Is The Future Of Glass In The Automobile

The history of the use of glass in cars is reviewed. New developments including electrochromic glasses and reaction injection moulding, and the possibility of replacing glass by plastic glazing, are discussed.

Author
L Colombin, L Jourdaine
Origin
Battelle Europe
Journal Title
Glass Digest June 15 1988 54-58