Initiation And Propagation Of Cracks In Glass Beneath A Disc Cutter

The distribution of mechanical stresses in glass under a disk cutter is investigated. The site of crack initiation in the glass is determined. It was established that a "mirror" zone appears under such conditions, and its size for the best edge to be formed in the glass determined. The stages of destruction of glass and disk cutter were determined.